Research Article

A Study on the Abrasion Resistance of Hydraulic Structures with Different Repair Mortars

Table 2

Properties of repair mortar materials.

S. No.Type of repair mortarPropertiesValues

(1)Silica fume mortarCompressive strength (at 28 days)85 MPa
Flexural strength (at 28 days)11 MPa
Hydraulic abrasion resistance index (at 28 days)Abraroc0.5–0.6
Glass1
Granite0.35–0.80
Wear resistance Bohme<6 cm3/50 cm2

(2)Polymer-modified mortarCompressive strength (at 28 days, +30°C)55 MPa
Flexural strength (at 28 days, +30°C)5 MPa