Material Characteristics and Electrical Performance of Perovskite Solar Cells with Different Carbon-Based Electrodes Mixed with CuSCN
Table 1
Compositions of the CuSN-incorporated electrode with different carbons.
| Electrode materials | Carbon (wt. %) | Oxygen (wt. %) | Copper (wt. %) |
| Bare activated carbon | 92.50 | 7.50 | 0.00 | CuSCN and activated carbon | 91.87 | 2.79 | 1.08 | CuSCN and CNT | 93.63 | 1.82 | 2.26 | CuSCN and graphite | 91.77 | 3.03 | 2.66 | CuSCN and GO | 63.80 | 19.57 | 11.58 | CuSCN and rGO | 65.86 | 13.97 | 13.14 |
|
|