Micro-CT scanning parameters.

ScaffoldMagnificationVoxel size (µm)Rotation step (°)Exposure time (s)Tube modeFrame averaging numberFrame skipped

Scaffold as-such10.00x5.000.501.5031
Scaffold soaked for 2 weeks in SBF11.11x4.500.501.5031