Table 1

the XRD parameters of (h k l), and d-value of standard wurtzite phase ZnO and samples.

(h k l)Int-fPCPDF79-0207 ZnOZnO/6GZnO/Sn ZnO/Sn /6G
d(nm)d(nm)d(nm)d(nm)d(nm)

(1 0 0)5700.282040.282200.282720.282200.28203
(0 0 2)4160.260620.261070.261510.260920.26078
(1 0 1)9990.248060.248200.248600.248200.24793
(1 0 2)2100.191410.191400.191630.191400.19133
(1 1 0)2910.162840.162680.162840.162680.16263
(1 0 3)2510.147930.147840.148010.147880.14835
(1 1 2)2030.138100.137960.138030.140820.14052