Nanocrystalline Diamond as a Coating for Joint Implants: Cytotoxicity and Biocompatibility Assessment

Figure 4

Cell viability/proliferation (a), total protein content (b), and ALP activity (c) of human bone marrow osteoblast cells grown on NCD-coated Si3N4 for 21 days. ∗ statistically different from the control.
894352.fig.004a
(a)
894352.fig.004b
(b)
894352.fig.004c
(c)