Research Article

Nanocrack Formation in Hematite through the Dehydration of Goethite and the Carbon Infiltration from Biotar

Figure 9

Observation of the rough surface by FE-SEM. (D: dense carbon layer, P: particle of carbon in low density).
235609.fig.009a
(a)
235609.fig.009b
(b)
235609.fig.009c
(c)
235609.fig.009d
(d)