Research Article
Mechanical and Fracture Behaviors of Elastomer-Rich Thermoplastic Polyolefin/ Nanocomposites
Table 1
Crystallization and thermal parameters for PP, ETPO blend and their composites.
| Sample | (°C) | (°C) | (J/g) | (%) |
| PP | 112.6 | 161.9 | 88.5 | 42.3 | PP/1 wt% | 116.8 | 162.0 | 87.6 | 42.3 | PP/3 wt% | 116.8 | 162.6 | 86.2 | 42.5 | PP/5 wt% | 118.4 | 162.5 | 85.6 | 43.1 | ETPO | 107.1 | 164.7 | 4.2 | 6.7 | ETPO-1 wt% | 107.6 | 164.5 | 2.0 | 3.2 | ETPO-3 wt% | 108.5 | 164.4 | 0.5 | 0.8 | ETPO-5 wt% | 108.5 | 164.8 | 0.5 | 0.8 |
|
|