Design and Preparation of Cross-Linked Polystyrene Nanoparticles for Elastomer Reinforcement

Figure 1

Morphology, size, and size distribution of cross-linked PS particles. (a) is the TEM image of cross-linked PS particles with DVB consumption of 20 wt% of styrene loading; (b) is the result of the same sample from the DLS test.
352914.fig.001a
(a)
352914.fig.001b
(b)