Research Article

Effect of Postdeposition Heat Treatment on the Crystallinity, Size, and Photocatalytic Activity of Nanoparticles Produced via Chemical Vapour Deposition

Figure 2

SEM micrographs (left) and respective nanoparticle size distribution histograms (right) for TiO2 nanoparticle samples deposited by CVD at (a) 400°C, (b) 500°C, (c) 600°C, and (d) 700°C.
512785.fig.002a
(a) sample 400°C
512785.fig.002b
(b) sample 500°C
512785.fig.002c
(c) sample 600°C
512785.fig.002d
(d) sample 700°C