Low-angle XRD patterns for porous ZnO film on ITO-glass from 0.05 M Zn(NO3)2 with 0.5 and 5 wt% SDS via electrodeposition and after soaking in water and ethanol for 2 days; and (b) Wide-angle XRD patterns for ZnO films on ITO-glass from 0.05 M Zn(NO3)2 with 0, 0.5 and 5 wt% SDS surfactants.