Research Article

Polyamic Acid Nanofibers Produced by Needleless Electrospinning

Figure 5

Thermogravimetric records of PI fibre (a) and PI film (b) (temperatures ( C ) corresponding to 5, 10,15, and 20 wt% weight loss are included).
842831.fig.005a
(a)
842831.fig.005b
(b)