Research Article

Regrowth of Carbon Nanotubes Array on Al Layer Coated Substrate

Figure 2

TEM images of CNT arrays grown after the (a) first, (b) second, and (c) third growth by the lift-off method, (d) second and (e) third growth by annealing method. (f) is the image of SWNTs bundle with the diameter of 0.86 nm after the third growth by annealing method.
906204.fig.002a
(a)
906204.fig.002b
(b)
906204.fig.002c
(c)
906204.fig.002d
(d)
906204.fig.002e
(e)
906204.fig.002f
(f)