Research Article

Precipitation of Zinc Oxide Nanoparticles in Bicontinuous Microemulsions

Figure 4

XRDPs for samples obtained from precipitation using 41.6% NaOH aqueous solution added by shooting (a) and at different dosing times: (b) 15; (c) 30; (d) 100 min. Standard patterns of Zn(NO3)2 (e) and ZnO (f) are included.
145963.fig.004