Crystal properties of TiO2-SiO2 oxide powder.

SampleTi/Si ratioSiO2 content (%)Final pH valueCrystallite size/nm (XRD)

SA01 : 0036.30
SA 519 : 1536.63
SA109 : 11037.06
SA165 : 116.6738.91
SA204 : 12039.54
SA253 : 12536.88
SA25-Cu(0.05)3 : 125310.8
SA25-Cu(0.1)3 : 12539.48
SA25-Cu(0.15)3 : 12539.62
SA25-Cu(0.2)3 : 125310.11
SA25-Cu(0.5)3 : 12538.21
SA25-53 : 12558.63
SN25-73 : 12579.98
SA307 : 330311.78
SA501 : 150311.76
SB01 : 0093.75
SB165 : 116.679
SB204 : 1209
SB253 : 1259
SB25-123: 12512
SB25-143 : 125144.57
SB307 : 3309
SB501 : 1509

SA: acid, SB: basic, SN: neutral.