Research Article

Determining Contact Angle and Surface Energy of Co60Fe20B20 Thin Films by Magnetron Sputtering

Figure 2

Contact images between 500 Å-thick CoFeB thin films and water as a test liquid under two sets of conditions: (a) deposited at RT; (b) postannealed at °C for 1 h.
291935.fig.002a
(a)
291935.fig.002b
(b)