Research Article

Growth Behaviors of ZnO Nanorods Grown with the Sn-Based Bilayer Catalyst-Covered Substrates

Figure 7

Surface morphologies of ZnO grown at 700°C for 2 h on (a) untreated, (b) 700°C preannealed, and (c) 850°C preannealed Sn/In substrates by thermal evaporation with a Zn mixture of Zn and ZnO in a weight ratio of 1 : 1. (d) EDS spectrum of the SEM image in (c).
603098.fig.007a
(a)
603098.fig.007b
(b)
603098.fig.007c
(c)
603098.fig.007d
(d)