Research Article

Characteristics of Progressive Damage of ZnO Nanowires during Contact Sliding under Relatively Low Loads

Figure 7

SEM image of the wear test under the load of (a) 2 mN, (b) 4 mN, and (c) 6 mN performed inside the SEM. Inset of triangle, arrow, and dotted regions show the large diameter, small diameter and compressed region of fractured ZnO nanowires, respectively.
624195.fig.007a
(a)
624195.fig.007b
(b)
624195.fig.007c
(c)