Thermal Behavior with Mechanical Property of Fluorinated Silane Functionalized Superhydrophobic Pullulan/Poly(vinyl alcohol) Blends by Electrospinning Method
Figure 1
DSC data of (a) PVA, (b) PULL/PVA blend membrane using electrospinning method (Applied voltage = 15 kV, TCD = 15 cm, Blend ratio (PULL/PVA) = 80/20, and Total polymer concentration = 9 wt.%), and (c) PULL.