Schematic drawings of an OLED (a) and OSC (b): thickness of the ITO electrode is 200 nm, the PEDOT+nc-TiO2 layer –100 nm, the MEH-PPV+nc-TiO2 layer –200 nm, for OLED and 300 nm for OSC, the thin TiO2 layer –30 nm, and the Al electrode –100 nm.