In Vitro Degradation of PHBV Scaffolds and nHA/PHBV Composite Scaffolds Containing Hydroxyapatite Nanoparticles for Bone Tissue Engineering

Figure 6

(a) Molecular weight (KDa) change with in vitro degradation time of PHBV scaffolds. (b) A plot of ln (molecular weight, KDa) with in vitro degradation of PHBV scaffolds for 44 weeks at 37°C; (minigraph) plot of ln (molecular weight, KDa) and degradation time (wk) at 37°C for 24 weeks.