Research Article

A Decrease in NiO-MgO Phase Through Its Solid Solution Equilibrium with Tetragonal ( L a 𝟏 βˆ’ 𝑧 S r 𝑧 ) 𝟐 N i 𝟏 βˆ’ 𝑦 M g 𝑦 O πŸ’ βˆ’ 𝛿 : Effect on Catalytic Partial Oxidation of Methane

Table 3

Coke deposited on the catalysts generated from the oxide mixtures: 0.4 La2O3–0.2 SrO–(1βˆ’x)NiO–xMgO after POM at 850Β°C over 50 h.

Different stoichiometry coefficient π‘₯ Coke on catalyst (wt%)

π‘₯ = 0 20.7
π‘₯ = 0 . 1 4.5
π‘₯ = 0 . 2 1.6
π‘₯ = 0 . 3 1.3
π‘₯ = 0 . 4 0.8
π‘₯ = 0 . 5 0.3