Effect of Alumina Dopant on Transparency of Tetragonal Zirconia

Figure 2

Dependence of the measured reflection of the yttria stabilized tetragonal zirconia without (3Y) and with alumina dopant (3YE). The thickness of these two samples was 1 mm.