Micromechanism and Kinetic Formulation of Vertically Aligned ZnO Nanorods Grown on Catalytic Bilayers

Figure 1

SEM images of one-dimensional ZnO grown at 700°C for 2 h on (a), (b) Sn, (c), (d) In, and (e), (f) Ni (a), (c), (e) sputter- or (b), (d), (f) spin coated silicon wafer substrates by thermal evaporation with a Zn mixture of Zn and ZnO in a weight ratio of 1.0 g : 1.0 g.