Research Article

Catalytic Activity of ZrO2 Nanotube Arrays Prepared by Anodization Method

Figure 2

The XRD patterns of zirconia nanotube arrays calcined at: (a) 200°C, (b) 400°C, (c) 600°C.
409571.fig.002