Research Article
Urea-Based Combustion Process for the Synthesis of Nanocrystalline Ni-La-Fe-O Catalysts
Figure 5
V-t plots for H2O2 decomposition obtained at 45°C over NiLaxFe2−xO4 catalysts calcined at 500°C, where (■), 0.50 (•),1.00 (▲), 1.50 (▼), and 2.00 (◄).