XRD patterns of CdS NC powders fabricated with different MPA concentrations (i) MPA/Cd2+ = 2.0/1.0 mol/mol, (ii) MPA/Cd2+ = 1.0/1.0 mol/mol, and (iii) MPA/Cd2+ = 0.5/1.0 mol/mol; solvent H2O/DMF = 0.2/1.0 w/w, reaction time 3 h. Inset shows the XRD pattern of CdS NC powder without addition of MPA.