Research Article

Engineered Hybrid Scaffolds of Poly(vinyl alcohol)/Bioactive Glass for Potential Bone Engineering Applications: Synthesis, Characterization, Cytocompatibility, and Degradation

Table 1

Pore size analyses of PVA/BaG/GA hybrids.

Concentration glutaraldehyde (GA, %)
0.01.05.05.0*

Medium pore size (μm)450490150
Maximum pore size (μm)11001000450450
Minimum pore size (μm)22018050100
Interconnections medium size (μm)7514535
Interconnections maximum size (μm)285475100200
Interconnections minimum size (μm)25351060

*Values obtained by micro-CT.