Research Article
Morphological Study on Room-Temperature-Cured PMMA-Grafted Natural Rubber-Toughened Epoxy/Layered Silicate Nanocomposite
Table 2
EDX analysis of all samples.
| | Atomic% (weight%) | Element | Epoxy | Epoxy-5 phr MG30 | Epoxy-5 phr Cloisite 30B | Epoxy-5 phr MG30-5 phr Cloisite 30B |
| C | 81.19 (76.41) | 81.72 (77.04) | 74.92 (67.45) | 73.21 (66.41) | O | 18.81 (23.59) | 18.28 (22.96) | 22.96 (26.69) | 25.41 (30.70) | Si | 0 | 0 | 1.98 (4.16) | 0.99 (2.10) | Al | 0 | 0 | 0.78 (1.57) | 0.33 (0.67) | Mg | 0 | 0 | 0.07 (0.13) | 0.07 (0.12) |
| Totals | 100 | 100 | 100 | 100 |
|
|