Time and Temperature Dependence of CdS Nanoparticles Grown in a Polystyrene Matrix
Figure 6
XRD spectra of CdS nanoparticles annealed at (a) 240°C and (b) 300°C. The vertical lines indicate the angular position of the reflections and in parenthesis are reported the Miller indices.