Research Article

Analysis of Large-Strain Extrusion Machining with Different Chip Compression Ratios

Figure 10

Distribution of strain through the primary deformation zone and the chip: (a) the location of the two trajectories AB and CD; (b) variation of effective strain along the trajectory AB in the primary deformation zone; (c) variation of strain through the thickness of the chip.
851753.fig.0010a
(a)
851753.fig.0010b
(b)
851753.fig.0010c
(c)