Research Article

On the Origin of Light Emission in Silicon Rich Oxide Obtained by Low-Pressure Chemical Vapor Deposition

Figure 6

Si–O stretching frequency positions for different Ro, for SRO films before and after annealing at 1,100°C for 180 minutes.