A Study on the Effect of Plasma Treatment for Waste Wood Biocomposites
Table 1
Contact angle and surface energy of PET film.
| Monomer | Contact angle (°) | Surface energy (dyne/cm) | Water | Glycerol | Total | Dispersion | Polar |
| Oxygen/PET | 8 | 9 | 73.73 | 12.78 | 60.96 | Benzene/PET | 58.8 | 65 | 49.17 | 1.08 | 47.37 | CH4/PET | 55.7 | 47.6 | 59.56 | 2.14 | 57.42 | Acrylic acid/PET | 35.7 | 47.7 | 71.94 | 1.72 | 70.22 | HMDSO/O2 (1 : 9)/PET | 28 | 41 | 75.74 | 2.54 | 73.21 | HMDSO/O2 (2 : 8)/PET | 56.5 | 60 | 47.25 | 4.32 | 42.93 | HMDSO/O2 (3 : 7)/PET | 66 | 68.8 | 38.03 | 4.39 | 33.64 | HMDSO/O2 (4 : 6)/PET | 72 | 73 | 32.39 | 4.57 | 27.81 | HMDSO/O2 (5 : 5)/PET | 73.5 | 73.5 | 30.64 | 5.43 | 25.21 | HMDSO/PET | 105 | 76 | 74.77 | 71.68 | 3.09 |
|
|