Research Article

Low-Temperature Annealing Induced Amorphization in Nanocrystalline NiW Alloy Films

Figure 4

Predicted dependence of upon for ranging from 0.22 to 0.28, with the two dashed lines representing the range of solubility limit (24 at.% to 30 at.%) for NiW alloys as reported in [28].
252965.fig.004