Reduction amplitudes of nano-GFRP immersed in water and alkaline solution.

Aging time (days)Water Alkaline solution
VE/clay nano-GFRPEP/clay nano-GFRPVE/clay nano-GFRPEP/clay nano-GFRP

150.54%3.11%11.20%4.22%
307.35%6.24%16.23%13.13%
4516.76%5.28%25.28%28.99%
6022.48%10.24%47.91%32.02%