Formation Behavior of Continuous Graded Composition in Ti-ZrO2 Functionally Graded Materials Fabricated by Mixed-Powder Pouring Method
Figure 7
SEM photographs of microstructure of Ti-ZrO2 FGMs for (A) sample A, (B) sample B, and (C) sample C. Photographs of (X-a), (X-b), (X-c) and (X-d) are taken at normalized position of 0.0 to 0.25, 0.25 to 0.5, 0.5 to 0.75, and 0.75 to 1.0, respectively.