Microhardness for the AA5083 samples prior to isothermal forging, where N0 represents the AA5083 initial material, N2 the ECAE processed AA5083 and N2 TT 340°C the ECAE processed AA5083 with the subsequent heat treatment at 340°C.

N0N2N2 TT 340°C

87.3123.7106.2
83.2140.698.2
86.3142.4112.7
76.0154.8103.0
87.4140.4103.7

Mean84.04140.38104.76