Figure 11

Fracture surface of the TiB2-B4C composite showing an agglomerate of TiB2 with a pore in the center, reactant mixture milled for 4 h, SPS-ed at 1600 (a); a nearly fully dense TiB2-B4C, reactant mixture milled for 16 h, SPS-ed at 1700 (b) (reprinted from [48], Copyright (2009), with permission from Elsevier).
625218.fig.0011a
(a)
625218.fig.0011b
(b)