Research Article

Reactive Spark Plasma Sintering: Successes and Challenges of Nanomaterial Synthesis

Figure 6

Fracture surface of Ti3SiC2-SiC nanocomposite SPS-ed at 1280°C showing grains of SiC about 100 nm in size, (a)—lower magnification, (b)—higher magnification (reprinted from [30], Copyright (2007), with permission from Elsevier).
625218.fig.006