Research Article

Self-Catalytic Growth of Tin Oxide Nanowires by Chemical Vapor Deposition Process

Figure 5

X-ray diffraction patterns of (a) pure SnO and (b) the as-synthesized SnO2 nanowires at a growth temperature of 1050°C for 30 min.
712361.fig.005a
(a)
712361.fig.005b
(b)