Research Article

Patterned Honeycomb Structural Films with Fluorescent and Hydrophobic Properties

Figure 2

(a) The fluorescence microscope image of the film before photopolymerization (left) and after photopolymerization (right); (b) fluorescent spectrum of the film before and after photopolymerization. Excitation: 320 nm. From the fluorescence microscope image and the fluorescent spectrum of the film before and after photopolymerization, it can be seen that the porous film can be prepared over a large area, which has the AIE property whether it is photopolymerizable or not.
853154.fig.002a
(a)
853154.fig.002b
(b)