A Mucoadhesive Electrospun Nanofibrous Matrix for Rapid Oramucosal Drug Delivery

Figure 5

(a) Linear rheological profile of 25%  PVA electrospinning solution, (b) thixotropy curve for the 25%  PVA solution used for electrospinning, (c) rheology plot depicting the yield stress (at 0.3782 Pa) of a 25%  PVA solution intended for electrospinning, and (d) stress sweep of 25%  PVA solution intended for electrospinning.