Research Article

Magnetic Properties and Microstructure of FeOx/Fe/FePt and FeOx/FePt Films

Figure 2

XRD patterns of FeOx(P)/Fe/FePt trilayer further annealed at 500°C with = (a) 1%, (b) 3%, and (c) 7% and 800°C with = (d) 1%, (e) 3%, (f) 7%.