Research Article

Optimization of the Electrodeposition Parameters to Improve the Stoichiometry of Films for Solar Applications Using the Taguchi Method

Table 5

Response table for signal-to-noise ratios.

Levels , deposition voltage (V) , deposition time (min) , composition of solution , deposition temperature (°C)

134.7931.6124.6825.04
223.2125.7330.9230.13
323.6324.5226.1527.18
11.587.086.235.10
Rank1234