Research Article

Synthesis and Characterization of Europium-Doped Zinc Oxide Photocatalyst

Figure 1

XRD patterns at of (a) 20°–75° and (b) 30°–38° of the as-synthesized undoped and Eu-doped ZnO samples synthesized by sonochemical method for 5 h.
367529.fig.001a
(a)
367529.fig.001b
(b)