Research Article
Preparation of Cd-Loaded In2O3 Hollow Nanofibers by Electrospinning and Improvement of Formaldehyde Sensing Performance
Table 1
Experimental parameters and characterized results.
| Sample | Cd·4H2O/In·4.5H2O (mg) | PVP (mg) | DMF/ethanol (mL) | Fiber diameter (nm) | Grain size (nm) |
| In2O3 | 0/764 | 917 | 5.6/7.0 | 156 | 26 | In20Cd1 | 30.8/764 | 954 | 5.8/7.3 | 52 | 19 | In10Cd1 | 61.6/764 | 1000 | 6.0/7.7 | 76 | 24 | In1Cd1 | 308/383 | 830 | 5.0/6.4 | 88 | 42 |
|
|