ICP-MS results of the latex rubber bands extract.

SampleZn (ppm)Ni (ppm)

GP-L8.45 ± 0.13a,bND
GP-3L7.95 ± 0.08aND
UN-L7.88 ± 0.21aND
UN-3L7.66 ± 0.14aND
EX-L7.53 ± 0.13a,bND
EX-3L5.78 ± 0.05aND
Control0.24 ± 0.01ND

Concentration of the “L” and “3L” samples from the GP, UN, and EX extracts.