Research Article
Cytotoxicity Comparison of the Nanoparticles Deposited on Latex Rubber Bands between the Original and Stretched State
Table 4
The concentration of the elements in the latex rubber bands (ppm).
| Sample | Fluoride | Chloride | Nitrate | Phosphate | Sulfate |
| GP-L | 17.64 ± 0.07 | 3992.08 ± 3.24 | 41.42 ± 0.16 | 444.57 ± 3.12 | 30.35 ± 0.27 | GP-3L | 17.83 ± 0.17 | 3986.18 ± 1.50 | 42.15 ± 0.13* | 450.52 ± 2.39 | 30.89 ± 0.19 | UN-L | 18.16 ± 0.07* | 4003.26 ± 7.87 | 42.87 ± 0.60 | 459.9 ± 7.69 | 31.57 ± 0.48* | UN-3L | 17.81 ± 0.05 | 3990.32 ± 7.05 | 41.45 ± 0.84 | 441.48 ± 8.24 | 30.34 ± 0.57 | EX-L | 17.29 ± 0.11 | 3984.58 ± 21.52 | 40.13 ± 0.99 | 429.54 ± 4.96 | 29.32 ± 0.71 | EX-3L | 17.35 ± 0.21 | 3990.82 ± 5.66 | 40.33 ± 0.81 | 432.47 ± 7.59 | 29.49 ± 0.60 | Control | 17.75 ± 0.34 | 3973.25 ± 15.07 | 41.73 ± 0.90 | 455.83 ± 9.61 | 30.36 ± 0.64 |
|
|
Concentration of the “L” and “3L” samples from the GP, UN, and EX extracts. compared with the control and 3L sample in each product.
|