Research Article

Evaluation of Degradation in Nanofilled Adhesive Resins Using Quantitative Light-Induced Fluorescence

Figure 4

QLF-D fluorescence images of (a, c, and e) pre- and (b, d, and f) postthermocycled resin disks. (a), (b) DR; (c), (d) SB; and (e), (f) GB.
671205.fig.004a
(a) Prethermocycling
671205.fig.004b
(b) Postthermocycling
671205.fig.004c
(c) Prethermocycling
671205.fig.004d
(d) Postthermocycling
671205.fig.004e
(e) Prethermocycling
671205.fig.004f
(f) Postthermocycling