Evaluation of Degradation in Nanofilled Adhesive Resins Using Quantitative Light-Induced Fluorescence
| Area | DR | SB | GB |
| 0 | | | | Prethermocycling | 4.3 ± 2.09a | 2.2 ± 0.1a | 20 ± 11.75a | Postthermocycling | 2.23 ± 2.10b | 1.78 ± 1.36a | 1.06 ± 1.6b | 70 | | | | Prethermocycling | 1.8 ± 1.46a | 1.9 ± 0.07a | 8.5 ± 8.84a | Postthermocycling | 0.05 ± 0.12b | 0.51 ± 0.80b | 0.05 ± 0.22b | 120 | | | | Prethermocycling | 0.9 ± 0.98a | 1.8 ± 0.06a | 3.2 ± 5.15a | Postthermocycling | 0 ± 0b | 0.40 ± 0.71b | 0 ± 0b |
|
|
Different lowercase letters indicate a significant difference between pre- and postthermocycling in each area ().
|