Research Article

The Phase and Morphology of Cu2ZnSnSe4 Nanopowders by Hydrothermal Method

Figure 3

The EDS results of Cu2ZnSnSe4 powders prepared at 200°C for different time. (a) 200°C for 45 h, (b) 200°C for 90 h.
(a)
(b)